Learn the common fusing problems in interlining, including bubbling, peeling, strike-through, shrinkage, and puckering, along with practical fixes to improve bonding quality and reduce production waste.
You fuse a batch of collars, and a few hours later you notice bubbles, peeling edges or a rippled surface. Rejections like this waste material and production time. The good news is that most fusing problems in interlining have clear causes and simple fixes.
Fusing bonds the interlining to the fabric using a heat-activated adhesive. For the bond to hold, heat, pressure and time must work together, and the interlining must suit the fabric. Here are the five most common problems.
Bubbles appear as raised, uneven patches on the fabric, often after fusing or the first wash.
Causes:
Fix: Lower the temperature slightly, increase pressure and check it is even across the panel, and dry the fabric before fusing.
Edges lift, corners peel, or layers separate after washing.
Causes:
Fix: Raise the temperature or extend the time within the fabric's limits, increase pressure, and choose an interlining suited to the fabric and its finish.
Strike-through is adhesive seeping to the face of the fabric, leaving shiny marks or stiffness. Strike-back is adhesive transferring onto the machine belt.
Causes:
Fix: Reduce heat and pressure, use a lighter adhesive coating on thin fabrics, and clean the machine belt regularly.
When fabric and interlining shrink at different rates, the garment ripples or puckers after washing or steaming.
Causes:
Fix: Test shrinkage on both materials before bulk cutting, choose an interlining with similar shrink behavior, and keep fusing temperature within the recommended range.
The bond is fine, but the garment feels too stiff or inconsistent from one area to another.
Causes:
Fix: Choose a lighter weight or softer finish, check that pressure is even edge to edge, and use different interlinings for different areas, such as one for collars and a softer one for plackets.
Knowing how to fuse interlining correctly means balancing three settings:
Exact settings vary by fabric and interlining, so follow your supplier's recommendations and test before every new combination.
Most fusing problems come from mismatched materials or wrong machine settings, and both are preventable with sample testing and technical support. A manufacturer that offers fusing process guidance can help you fine-tune your line and avoid rework.
Facing bubbling or adhesion issues on your line? Contact JGS Tex Fab for technical support and samples.
Please have the client confirm the technical guidance before publishing, since ideal settings depend on their products. I can also write another title from the list, such as Interlining for Shirts or Buckram vs Microdot.
Keep reading
3 min readDiscover the role of non-woven fabric in embossing and precision cutting, from improved material stability to better production consistency.
Read the article
3 min readEmbroidery backing paper is the hidden layer that decides whether an order ships or gets stitched twice. Here’s what it is, the four main types, and how to choose the right one for your fabric.
Read the article
2 min readUnderstand how OEKO-TEX certification helps garment brands meet buyer expectations, improve material safety assurance, and choose reliable interlining and non-woven fabric for quality-conscious apparel production.
Read the articleLet's Connect
Tell us the fabric, the garment and the run size. We will come back with the interlining that fits, and a sample to prove it.
Send an enquiry